Demand Submission
Please leave us a message and we will contact you within 24 hours
PRODUCTS
Specializing in the production of highquality silicone rubber products
PRODUCT
Specializing in the production of highquality silicone rubber products
— Product Categories
Silicone tube
LED light strip silicone sleeve
Foamed silicone tube
Silicone braided tube
Medical silicone tube
Peristaltic pump silicone hose
Communication/power shrink tubing
Silicone shielding strip
Foam silicone sealing strip
Silicone sealing strip/ring
Bicycle handle cover/strap
Silicone sheets and miscellaneous parts
Silicone leather
— News Recommended
top Introducing the Innovative Foam Silicone Tube:...
top Enhancing the Lifespan of High-Temperature Sil...
top Colored Silicone Tube: Production Process and ...
Custom Silicone Foam Tube: Sizes, Colors, and ...
UL94 V-0 Silicone Foam Tube for EV Battery Pro...
Food Grade Silicone Foam Insulation Tube: FDA ...
Silicone Foam Tube vs EPDM Rubber Foam: Which ...
Platinum-Cured vs Peroxide-Cured Silicone Foam...
— Products Recommended

Braided silicone tube for ice makers: an inner-braid three-layer build (food-grade silicone bore, braid, silicone skin) that keeps a 2.0 mm wall from collapsing on the pump suction line. ID 4–12 mm common, −40 to +200 °C, working pressure quoted per section against the safety factor, NSF/ANSI 51 and FDA 21 CFR 177.2600 materials.
An ice machine fills, circulates and drains the same water all day. On the fill and circulation runs the pump pulls more than it pushes, and a thin silicone wall has only its own hardness to stop it closing. This tube puts a braid between the bore and a silicone skin, so the bore keeps the diameter it was extruded at.
Inner braid, 3 layersID 4–12 mm commonNSF/ANSI 51 materials−40 °C to +200 °CCustom sectionsThree layers: a food-grade silicone bore, one braid layer wound over it, and a silicone outer skin. No adhesive or bonding layer touches the water — the braid is wound onto the tube, not laminated into it.
Food-grade silicone, smooth and non-porous. Wall thickness follows the bore and the duty.
Wound at a set angle and coverage; takes the inward pull on suction and the hoop load under pressure.
Silicone over the braid: keeps yarn away from cleaner and moisture, stops the cut end fraying, and wipes down.
The split is by what the water is doing, not by the price of the machine. Five runs, and only the first three repay a braid. Sections and braid options across the whole range are on the braided silicone hose page.
| Run | Typical condition | Braid? | Why |
|---|---|---|---|
| Water inlet → reservoir or float valve | building water, 0.13–0.8 MPa | Yes, on long or tight runs | Pressure is low but the run is long; the braid stops the wall ballooning at the joints. |
| Reservoir → pump → evaporator (suction) | below atmospheric | Yes — the critical one | The load is inward, and a thin wall creeps closed a little on every cycle. |
| Circulation return from the evaporator | 0–5 °C water, low pressure | Usually | Cold water and a bend all day; braid resists flattening at the bend. |
| Drain and overflow | tank pressure, open outlet | No | Nothing to resist, and a technician may need to see whether it drains. |
| Water-cooled condenser feed | line pressure, warm side | Optional | Only where the route collapses or the tube is a structural run. |
Between reservoir and pump the pressure is below atmospheric for most of the cycle, so every stroke pulls the wall inward. Silicone returns to shape well but not perfectly: over thousands of strokes the bore takes a set, narrows, and the pump moves less water without sounding any different.
What shows up is not a burst. It is ice thin at the end of a sheet and a harvest cycle running past the timer. Three things worth checking on a tube that has been in service:
Cut a section and hold it against a rule. An oval or a flattened band means the wall was doing the braid's job.
Thinning concentrates at the shortest radius in the cabinet, not on the longest run.
A tube that has grown under cycling also grows at the joint — a clamp question, not a braid one.
Where the braid sits decides two things at once: what the outside of the tube is, and how the colour gets in.
Yarn is the outer surface, so colour goes on as a pigment paste over exposed yarn. Paste carries odour, normally handled with a second vulcanising pass — and odour is what a food-contact review asks about. That is why an external braid build usually cannot carry an NSF statement.
The braid sits under a silicone skin and the colour goes in as a food-grade silicone compound, not a paste on yarn. No exposed yarn, no paste: the inner-braid construction is the one that can be documented to NSF/ANSI 51 as material for food equipment.
That is a materials statement, not a certificate for the part. Material documents ship with the order, product-level testing is arranged per project, and the certificate for the assembled machine sits with the machine builder.
| Standard | What it covers | Where it sits for this part |
|---|---|---|
| NSF/ANSI 12 | Ice-making equipment (the machine) | Not ours to hold — it applies to the builder's product. |
| NSF/ANSI 51 | Food equipment materials | The level our silicone and colour compound are documented against. |
| NSF/ANSI 61 | Drinking-water system components | A different test; relevant only if the line is a potable-water component. |
We send FDA 21 CFR 177.2600 and LFGB statements, REACH and RoHS declarations and NSF/ANSI 51 material documentation with the shipment; the plant runs ISO 9001 and ISO 13485, and batches trace from compound to finished coil. The tube is not for human implantation.
The ranges below are what machine builders publish for their own units: a starting point, not a specification of the tube. Quote against the run, not against a machine class.
| Point in the circuit | Typical figure | What it means for the tube |
|---|---|---|
| Water inlet | 0.13–0.8 MPa; most machines 0.15–0.5 MPa | City or building pressure, so the fill line is rarely the critical run. |
| Inlet water temperature | 5–35 °C | Cold water, which is why 200 °C of material headroom stays unused. |
| Circulating water over the evaporator | 0–5 °C | The coldest continuous duty, and the one that sets the braid choice. |
| Wash / rinse / sanitise | 15 / 15 / 25 minutes, repeated daily | Short warm peaks and a chemical load; this ages the tube, not heat. |
| Pump suction side | below atmospheric | The load is inward — not a pressure rating in the usual sense. |
Almost every enquiry asks about heat. Almost every failure comes from cycling: cold water on and off with a warm wash between, hundreds of times a month. Freeze-thaw is where a bore changes — water left in a line, a machine standing in an unheated space, a defrost that outruns the drain. The braid is what keeps that load from becoming a permanent change of shape. On the chemical side it is concentration creep and dwell time that shorten life, not the sanitiser at the strength a machine uses.
Bore is quoted as ID and the wall follows from the duty. Published sections across the braided range run 3 mm to 31.75 mm ID; the four bands below are the ones on ice machine drawings. Where a run needs more headroom than a single braid gives, the double-layer mesh build is the next step up.
| Section (ID) | Where it turns up | Note |
|---|---|---|
| 4–5 mm | Small under-counter and domestic machines; evaporator in and out | The tight-bend end of the range — check the run before stepping up a size. |
| 6–8 mm | The mainstream: pump suction and water circulation | Most replacement parts sit here. A 6 mm bore is not a 1/4 inch line. |
| 8–10 mm | Commercial machines with longer runs | Bending radius decides the wall; check it before stepping down. |
| 10–12 mm | Drain and overflow lines | Usually the run that does not need a braid at all. |
Walls across these sections run 2.0–3.0 mm. The thin end is what makes a suction run worth braiding: flexible enough for a small cabinet, thin enough that unbraided it takes a set under a pump. Going thicker instead buys burst strength and loses flexibility, which reappears as assembly stress at the joints.
A 1/4 inch line is 6.35 mm, so a 6 mm bore is not the same part and will not seal the same way on a 1/4 inch barb. The others that come up: 5/32 inch is 3.97 mm, 5/16 inch is 7.94 mm, 3/8 inch is 9.53 mm. Ask which system the drawing came from before quoting — this is the most common mismatch on a replacement order.
Burst pressure is quoted per section. Across the published braided range the figures run 1.18–3.73 MPa, and your drawing gets its own number rather than a range.
Working pressure is not a property of the tube on its own: it is the burst figure divided by the safety factor the machine is designed to, 4:1 for general duty and 3:1 where a shorter service interval is accepted. On the suction side the load reverses, so a burst figure says nothing useful — the braid is what resists collapse, and how much a construction takes is quoted per construction. A wall thick enough to resist collapse by itself is also stiff enough to fight a small cabinet.
Four cases where the braid costs money and buys nothing:
Braid is opaque. Where a technician diagnoses by looking for bubbles, scale or a slow drain, a clear tube does it better.
Drain, overflow and open outlets have nothing to resist; a braid hides the flow without adding life.
Under about 20 mm the braid adds stiffness and makes assembly harder for no gain.
Repeated plugging works the cut end; an unbraided tube with a clean cut is the honest choice.
A secondary refrigerant is chosen for heat transfer, not for taste, so the answers differ from potable water — and in order of how confident we are:
Food-grade heat-transfer fluid, common in ice machines. Silicone is compatible; this is the case we support from material data.
Compatible with the silicone, but the fluid is toxic: the tube is fine, the leak path is the risk. Say what the circuit is and the wall is set accordingly.
Not recommended without a test on the actual fluid. Chloride finds its way into a cut end; send a brine sample and we run it rather than guess.
Built to the drawing, not chosen from a list: wall 2.0–3.0 mm across the ice machine bands.
Polyester as standard for cold water, aramid where a line also runs hot; angle and coverage set at the winder.
Food-grade silicone compound matched to a sample or code, with bare ends for your own barb or clamp; non-silicone fittings are integrated through partner manufacturers — we make the silicone part.
Coils, spools or straight lengths labelled per line item, with material statements and declarations in the box.
The tube is the last step of a chain controlled from the compound up: Guilin Yutian New Materials (compound, 28,000 m²), Dongguan Huahong Rubber and Plastic (compounding and batch control) and Dongguan Yutian Silicone (extrusion, braiding and finishing in a 6,800 m² plant) — 14 extrusion lines, 4 calendering lines and 7 moulding presses in a Class 100,000 cleanroom, up to 8 million metres a month, since 2012.
Most ice machine enquiries take three or four rounds because the drawing and the duty are not in the first message. This list usually does it in one.
| What we need | What to send | Why it matters |
|---|---|---|
| Machine and position | Model, and where in the circuit the tube sits | Decides temperature, pressure and whether the run is under suction |
| Section | ID × OD, or ID plus wall | 1/4 inch is 6.35 mm, not 6 mm |
| Water pressure | Inlet pressure and the pump-side figure | An inlet range and a suction run are not the same specification |
| Temperature and cleaning | Water temperature and the wash / sanitise routine | Decides the compound and whether aramid braid is needed |
| Medium | Potable water, glycol, or brine with its chemistry | Brine needs a compatibility answer, not an assumption |
| Length, ends and quantity | Cut length and tolerance, barb or clamp, per-release volume | Sets the cutting and packing method |
Without all of it, send a photo of the original tube, the machine model and the position. Standard sections ship in 5 to 7 working days, stock samples in 3 days, a custom construction in 10 to 20 working days; samples are free and freight is paid by the buyer. The same construction questions on the hot side are set out on the coffee machine tube page.
Does an ice machine need a braided hose at all?
On three runs: inlet, pump suction and the circulation return. On drain and overflow, no — the line sits at tank pressure and an opaque wall only makes a slow drain harder to diagnose.
Why would a silicone tube collapse on the suction side?
The load is inward and a thin wall has only its own hardness to hold the bore. Silicone returns to shape well but not perfectly, so a 2 mm wall takes a set and the flow drops without the pump sounding any different.
What is different about an inner braid?
Where the yarn sits. An external braid is the outer surface, so it takes abrasion and the colour sits on exposed yarn. An inner braid is covered by a silicone skin: wipeable outside, no fraying at the cut, and colour as a food-grade compound.
Can this tube carry an NSF statement?
The silicone and colour compound are documented to NSF/ANSI 51 as materials for food equipment, and the documents ship with the order. That is material level; a product-level report is arranged per project, and the machine certificate sits with the builder.
What temperature does it take?
−40 °C to +200 °C continuous. In an ice machine the interesting end is the cold one: 0–5 °C circulating water and daily wash cycles are what age the tube.
Can it carry glycol or brine?
Propylene glycol we support from material data, ethylene glycol is compatible but toxic, and chloride brines we will not recommend without testing the actual fluid.
Which sections do you keep in stock?
The 6–8 mm band covers most replacement orders. Published sections run 3 mm to 31.75 mm ID, and anything between is made to the drawing.
What about lead time and samples?
Standard sections ship in 5 to 7 working days, stock samples in 3 days, custom construction in 10 to 20 working days. Samples are free; freight is paid by the buyer.
Send the machine model, the section and the position in the circuit. You get the section review, the burst figure for that run and a sample date back.
Request a quoteWhatsApp +86 18028921514 · salesmanager@yutiansilicone.com

Copy product links
Long by picture save/share


— News Recommended
top Introducing the Innovative Foam Silicone Tube: A High-Perfor...
top Enhancing the Lifespan of High-Temperature Silicone Tubes in...
top Colored Silicone Tube: Production Process and How to Choose
Custom Silicone Foam Tube: Sizes, Colors, and Specifications...
UL94 V-0 Silicone Foam Tube for EV Battery Protection: Safet...
Food Grade Silicone Foam Insulation Tube: FDA Compliance and...
— Products Recommended
Message
Hi!If you are looking for custom-made silicone rubber products, feel free to ask me any questions.